Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.60 - 5.20 µm/m-°C @Temperature 20.0 - 400 °C |
2.56 - 2.89 µin/in-°F @Temperature 68.0 - 752 °F |
|
Special Metals NILO® Alloy K Controlled-Expansion Alloy Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat.. |