Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.2 - 16.2 µm/m-°C @Temperature 20.0 - 100 °C |
8.44 - 9.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 0.000 - 800 °C |
8.44 µin/in-°F @Temperature 32.0 - 1470 °F |
|
Kennametal Stellite Stellite® 12 PM with P/M Processing Applications: include vane plugs, fuel metering pins, spacer bushings, ball blanks (bearings), race blanks (bearings), diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wea.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 188 alloy, hot rolled and 1175°C solution annealed plate Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 188 alloy, plate at RT after 4000 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 188 alloy, plate at RT after 8000 hours at 650°C (1200°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 214® alloy, 20% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 214® alloy, 40% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 214® alloy, 50% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 800 °C |
8.44 µin/in-°F @Temperature 77.0 - 1470 °F |
|
Haynes 230® alloy, 10% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 800 °C |
8.44 µin/in-°F @Temperature 77.0 - 1470 °F |
|
Haynes 230® alloy, 10% cold reduction, 1121°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 800 °C |
8.44 µin/in-°F @Temperature 77.0 - 1470 °F |
|
Haynes 230® alloy, 10% cold reduction, 1177°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 800 °C |
8.44 µin/in-°F @Temperature 77.0 - 1470 °F |
|
Haynes 230® alloy, 20% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 800 °C |
8.44 µin/in-°F @Temperature 77.0 - 1470 °F |
|
Haynes 230® alloy, 30% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 800 °C |
8.44 µin/in-°F @Temperature 77.0 - 1470 °F |
|
Haynes 230® alloy, 30% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 0.000 - 900 °C |
8.44 µin/in-°F @Temperature 32.0 - 1650 °F |
|
Kennametal Stellite Stellite® 12 Satisfactory finishing results can be obtained using carbide tipped tools. Applications include cutting plastics, rubber, paper, carpet, and wood; saw teeth, trimmer knives, carpet knives, ledger bl.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 188 alloy, plate at RT after 8000 hours at 760°C (1400°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 214® alloy, 10% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 600 °C |
8.44 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes 214® alloy, 30% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 800 °C |
8.44 µin/in-°F @Temperature 77.0 - 1470 °F |
|
Haynes 230® alloy, plate, 8000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 500 °C |
8.44 µin/in-°F @Temperature 77.0 - 932 °F |
|
Osprey Metals CE13 Al-Si Controlled Expansion Alloy Al-42%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 800 °C |
8.44 µin/in-°F @Temperature 77.0 - 1470 °F |
|
Haynes 230® alloy plate, 16000 hours exposure at 649°C (1200°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 800 °C |
8.44 µin/in-°F @Temperature 77.0 - 1470 °F |
|
Haynes 230® alloy plate, 8000 hours exposure at 649°C (1200°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 800 °C |
8.44 µin/in-°F @Temperature 77.0 - 1470 °F |
|
Haynes 230® alloy, 50% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
CTE, linear | 15.2 µm/m-°C @Temperature 25.0 - 800 °C |
8.44 µin/in-°F @Temperature 77.0 - 1470 °F |
|
Haynes 230® alloy, 50% cold reduction, 1121°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |