Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.7 µm/m-°C @Temperature 25.0 - 100 °C |
8.16 µin/in-°F @Temperature 77.0 - 212 °F |
|
Carlson 20 Plus Alloy Carlson C20 Plus is a super-austenitic alloy, developed to provide maximum resistance to corrosion by sulfuric acid. Nickel chromium, molybdenum and copper contribute to the excellent overall resist.. |