Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.2 µm/m-°C @Temperature 20.0 - 199 °C |
7.90 µin/in-°F @Temperature 68.0 - 390 °F |
|
Carlson 2205 (UNS S31803) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
CTE, linear | 14.2 µm/m-°C @Temperature 20.0 - 199 °C |
7.90 µin/in-°F @Temperature 68.0 - 390 °F |
|
Carlson 2205 (UNS S32205) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
CTE, linear | 14.2 µm/m-°C @Temperature 21.1 - 316 °C |
7.90 µin/in-°F @Temperature 70.0 - 600 °F |
|
Carlson C 600 Nickel-Chromium-Iron Alloy Carlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excellent resistance to c.. |
|||
CTE, linear | 14.2 µm/m-°C @Temperature 21.1 - 316 °C |
7.90 µin/in-°F @Temperature 70.0 - 600 °F |
|
Carlson C 600ESR Nickel-Chromium-Iron Alloy General DescriptionCarlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excell.. |