Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.7 µm/m-°C @Temperature 21.0 - 204 °C |
7.60 µin/in-°F @Temperature 69.8 - 399 °F |
|
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 21.1 - 538 °C |
7.60 µin/in-°F @Temperature 70.0 - 1000 °F |
|
Crucible Steel CSM® 2 Mold Steel, AISI P20 CSM 2 is a prehardened, general purpose mold steel suitable for production of machined or EDM’d plastic mold and zinc die casting die components. CSM 2 is supplied prehardened at two hardnesses: re.. |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 21.1 - 649 °C |
7.60 µin/in-°F @Temperature 70.0 - 1200 °F |
|
Crucible Steel LABELLE® Silicon #2 Tool Steel LaBelle Silicon #2 is a shock resisting tool steel capable of maximum toughness at relatively high hardness. It has excellent resistance to impact and battering, with good edge retention.Information.. |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 20.0 - 100 °C |
7.60 µin/in-°F @Temperature 68.0 - 212 °F |
|
Carlson 2205 (UNS S31803) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 20.0 - 100 °C |
7.60 µin/in-°F @Temperature 68.0 - 212 °F |
|
Carlson 2205 (UNS S32205) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 21.1 - 427 °C |
7.60 µin/in-°F @Temperature 70.0 - 800 °F |
|
Carlson C 625 Nickel-Chromium-Molybdenum Alloy General DescriptionCarlson Alloy C 625 is a nickel-chromium-molybdenum alloy that combines high strength and oxidation resistance with excellent corrosion resistance. C 625 exhibits exceptional fat.. |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 100 °C |
7.60 µin/in-°F @Temperature 212 °F |
|
ATI Wah Chang Tiadyne™ 3510 Capable of being surface hardened to depths that produce very high wear resistance. Produced by traditional metallurgical processing, not special treatments.Information provided by ATI Wah Chang |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 21.1 - 302 °C |
7.60 µin/in-°F @Temperature 70.0 - 575 °F |
|
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared t.. |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 21.1 - 302 °C |
7.60 µin/in-°F @Temperature 70.0 - 575 °F |
|
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel Description: Formadur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared .. |