Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.58 µm/m-°C @Temperature 38.0 - 649 °C |
6.989 µin/in-°F @Temperature 100 - 1200 °F |
|
Latrobe TNWâ„¢ ASTM M10 High Speed Steel TNW is an M10 type high speed steel with a composition that combines the high toughness of a high-molybdenum steel and the excellent wear resistance provided by the 2%
vanadium content. TNW is popul.. |