Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.56 µm/m-°C @Temperature 21.0 - 300 °C |
6.978 µin/in-°F @Temperature 69.8 - 572 °F |
Mean |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.250 in (6.4 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.250 inch plate. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
CTE, linear | 12.56 µm/m-°C @Temperature 21.0 - 300 °C |
6.978 µin/in-°F @Temperature 69.8 - 572 °F |
Mean |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.500 in (12.7 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.500 inch plate. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
CTE, linear | 12.56 µm/m-°C @Temperature 21.0 - 300 °C |
6.978 µin/in-°F @Temperature 69.8 - 572 °F |
Mean |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Round 1.500 in (38.1 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 1.500 inch round. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
CTE, linear | 12.56 µm/m-°C @Temperature 21.0 - 300 °C |
6.978 µin/in-°F @Temperature 69.8 - 572 °F |
Mean |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.062 in (1.6 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.062 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
CTE, linear | 12.56 µm/m-°C @Temperature 21.0 - 300 °C |
6.978 µin/in-°F @Temperature 69.8 - 572 °F |
Mean |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.125 in (3.2 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.125 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufacture.. |