Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.0 µm/m-°C @Temperature 400 °C |
6.67 µin/in-°F @Temperature 752 °F |
|
Outokumpu 4028 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 600 °C |
6.67 µin/in-°F @Temperature 1110 °F |
|
Outokumpu 4762 High Temperature Ferritic Stainless Steel Highest chromium content-most resistant to reducing sulphurous gases. Susceptible to 475°C embrittlement and s-phase forms during long exposures in the range 600-800°C.Applications: Mostly used i.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 100 - 200 °C |
6.67 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 300 °C |
6.67 µin/in-°F @Temperature 68.0 - 572 °F |
|
Kennametal Stellite Nucalloy® 453 High-Silicon Nickel-Base Hardfacing Alloy Applications include chemical control valves, nuclear globe valves, nuclear gate valves, nuclear sliding parts, and pressure bars for plywood cutters.Nucalloy® alloys are unique, patented, high-s.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 38.0 - 200 °C |
6.67 µin/in-°F @Temperature 100 - 392 °F |
|
Latrobe LSSâ„¢ Vertex Tool Steel TLS Vertex tool steel is a versatile, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, chromium-rich alloy carbides in the micros.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 24.0 - 204 °C |
6.67 µin/in-°F @Temperature 75.2 - 399 °F |
|
HP Alloys Alloy C-276, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.67 µin/in-°F @Temperature 68.0 - 392 °F |
|
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.67 µin/in-°F @Temperature 68.0 - 392 °F |
|
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.67 µin/in-°F @Temperature 68.0 - 392 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 600 °C |
6.67 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Carpenter Chrome Core® 12 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 22.0 - 482 °C |
6.67 µin/in-°F @Temperature 71.6 - 900 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 300 °C |
6.67 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter HyMu "80"® Electronic Alloy, Bar, After Process Anneal Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.67 µin/in-°F @Temperature 68.0 - 392 °F |
200 HB |
Assab Steels 760 Machinery Steel ASSAB 760 is an easily machinable carbon steel characterized by: Good machinabilityGood mechanical strengthASSAB 760 is primarily intended to be used in the as-delivered condition. It is only to be .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy Characteristics: non-age hardenable; outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress corrosion cracking; high strength; high du.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 500 °C |
6.67 µin/in-°F @Temperature 68.0 - 932 °F |
|
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire, bar, and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
CTE, linear | 12.0 - 14.0 µm/m-°C @Temperature -40.0 - 125 °C |
6.67 - 7.78 µin/in-°F @Temperature -40.0 - 257 °F |
X/Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |