Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Kennametal Stellite Stellite® 98M2 cast Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Kennametal Stellite Stellite® 98M2 with P/M Processing Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 21.0 - 427 °C |
6.50 µin/in-°F @Temperature 69.8 - 801 °F |
|
Latrobe Lescalloy® 15-5 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 15-5 VAC-ARC steel is a precipitation hardening martensitic stainless steel commonly considered to be a compositional modification of 17-4 with minimal delta ferrite. A wide range of mec.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 21.0 - 427 °C |
6.50 µin/in-°F @Temperature 69.8 - 801 °F |
|
Latrobe Lescalloy® 17-4 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe LSSâ„¢ 420 MQ Plastic Mold Steel (AISI 420) TLS 420 MQ is a highly-refined, Mold Quality stainless steel that is engineered to exhibit excellent polishability, good corrosion resistance, and good wear resistance. TLS 420 MQ is melted using an.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 500 °C |
6.50 µin/in-°F @Temperature 932 °F |
upon cooling |
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Industeel CLC 1.2316S Prehardened Mold Steel (300HB) with Improved Machinability Description: CLC 1.2316 S grade is a 16%Cr 1%Mo mold steel with improved corrosion resistance properties, thanks to the chromium and molybdenum additions. Furthermore specific sulfur additions are c.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 100 °C |
6.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
HP Alloys Alloy C-276, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 100 °C |
6.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
HP Alloys Alloy C-276, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 100 °C |
6.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
HP Alloys Alloy C-276, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 1000 °C |
6.50 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec MZ 111 HIP Zirconia, ZrO2-Y2O3 MZ 111 HIP is a yttria-stabilized tetragonal zirconia ceramic. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 1000 °C |
6.50 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec MZ 111 Zirconia, ZrO2-Y2O3 MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 399 °C |
6.50 µin/in-°F @Temperature 68.0 - 750 °F |
|
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel Ultrachem® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by: exceptional corrosion resistance, uniform hardness in all dimensions, .. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 0.000 - 100 °C |
6.50 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel Uddeholm Mirrax ESR is specially developed and adapted for larger molds that require corrosion resistance and/or high surface finish.It is characterized by:High hardenability for consistent properti.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 399 °C |
6.50 µin/in-°F @Temperature 750 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel Uddeholm Vanadis 30 is a Co high alloyed powder metallurgy high speed steel corresponding to AISI M3:2 + Co. The high compressive strength, 67 HRC, and good abrasive wear resistance makes Uddeholm V.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 399 °C |
6.50 µin/in-°F @Temperature 750 °F |
hardened to 60 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature <=427 °C |
6.50 µin/in-°F @Temperature <=801 °F |
|
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 900 AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature -17.8 - 300 °C |
6.50 µin/in-°F @Temperature 0.000 - 572 °F |
|
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Assab Steels VANADIS 10 Cold Work Steel VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:Extremely high abrasive wear resistanceHigh compressive strengthVery good through-hardening propertiesGood toughne.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature <=427 °C |
6.50 µin/in-°F @Temperature <=801 °F |
|
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 100 °C |
6.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
HP Alloys Alloy C-276, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 100 °C |
6.50 µin/in-°F @Temperature 68.0 - 212 °F |
Annealed |
Schmolz + Bickenbach Cryodur® 2767 Cold Work Die Steel Description: High hardenability and toughness, highly suitable for polishing, texturing and EDM machining. We recommend the use of Cryodur® 2767 (ERS) for extreme demandsApplications: Cutlery dies,.. |