Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 107 µm/m-°C @Temperature 0.000 - 20.0 °C |
59.4 µin/in-°F @Temperature 32.0 - 68.0 °F |
T<Tg; ASTM E831-93 |
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu.. |
|||
CTE, linear | 107 µm/m-°C @Temperature <=150 °C |
59.4 µin/in-°F @Temperature <=302 °F |
ISO E 831 |
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
CTE, linear | 107 µm/m-°C @Temperature 0.000 - 20.0 °C |
59.4 µin/in-°F @Temperature 32.0 - 68.0 °F |
T<Tg; ASTM E831-93 |
3D Systems Accura® 25 Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el.. |