Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.5 µm/m-°C @Temperature 25.0 - 300 °C |
5.83 µin/in-°F @Temperature 77.0 - 572 °F |
|
Osprey Metals CE9 Al-Si Controlled Expansion Alloy Si-40%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 400 °C |
5.83 µin/in-°F @Temperature 752 °F |
|
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 100 °C |
5.83 µin/in-°F @Temperature 212 °F |
|
Outokumpu 4021 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 100 °C |
5.83 µin/in-°F @Temperature 212 °F |
|
Outokumpu 4028 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 800 °C |
5.83 µin/in-°F @Temperature 1470 °F |
|
Plansee CFY Chromium-Iron-Yttrium The most typical use for CFY is as interconnects in fuel cells.Characteristics: Coefficient of expansion - designed for compatibility with that of the electrolyte in fuel cells Corrosion resistance.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 100 °C |
5.83 µin/in-°F @Temperature 68.0 - 212 °F |
|
Latrobe LSSâ„¢ 420 HC High Carbon Stainless Steel TLS 420 HC is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 55 HRC and good wear resistance. TLS 420 HC should be considered for applications such .. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 100 °C |
5.83 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT550 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 300 °C |
5.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott FG13 Conversion Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BG34, FG3 |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 300 °C |
5.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott GG475 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG385, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 300 °C |
5.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott WG225 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 300 °C |
5.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF1 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 300 °C |
5.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott GG435 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG385, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 300 °C |
5.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott RG1000 Long Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 21.0 - 93.0 °C |
5.83 µin/in-°F @Temperature 69.8 - 199 °F |
|
Crucible Steel CPM® 15V® Tool Steel CPM 15V is intended for applications requiring exceptional wear resistance. It has more vanadium carbides in its microstructure than CPM 10V and provides more wear resistance and longer tool life in.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 100 °C |
5.83 µin/in-°F @Temperature 68.0 - 212 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 200 °C |
5.83 µin/in-°F @Temperature 392 °F |
|
Bohler-Uddeholm BÖHLER S590 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 100 °C |
5.83 µin/in-°F @Temperature 68.0 - 212 °F |
|
Carpenter No. 610® High Carbon, High Chrome Tool Steel (Air-Wear) (AISI D2) No. 610 tool steel is an air hardening, high-carbon, high-chromium tool steel having extremely high wear resisting properties. It is very deep hardening, and will be practically free from size chang.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 200 °C |
5.83 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum 410 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 25.0 - 600 °C |
5.83 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 843°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 25.0 - 600 °C |
5.83 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 25.0 - 600 °C |
5.83 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Carpenter Hiperco® Alloy 50 Fe-Co-V Soft Magnetic Alloy, Cold Rolled Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 25.0 - 600 °C |
5.83 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 200 °C |
5.83 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 204°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 200 °C |
5.83 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 288°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 200 °C |
5.83 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 482°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 100 °C |
5.83 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |
|||
CTE, linear | 10.5 µm/m-°C @Temperature 20.0 - 100 °C |
5.83 µin/in-°F @Temperature 68.0 - 212 °F |
|
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corr.. |