Thermal Properties Metric English Comments
CTE, linear 10.44 µm/m-°C

@Temperature 24.0 - 260 °C
5.800 µin/in-°F

@Temperature 75.2 - 500 °F
Carpenter Custom 450® Stainless Steel, Annealed
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
CTE, linear 10.44 µm/m-°C

@Temperature 20.0 - 100 °C
5.800 µin/in-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum AL 433™ Ferritic Stainless Steel, Annealed
AL 433™ is a stainless steel in the ferritic family of alloys with Type 409 and Type 439. The AL 433 alloy contains 20% chromium for pitting and crevice corrosion resistance in the presence of chl..