Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 300 °C |
5.67 µin/in-°F @Temperature 68.0 - 572 °F |
|
Kennametal Stellite Delcrome® 93 Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 100 °C |
5.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
Latrobe LSSâ„¢ 420 MQ Plastic Mold Steel (AISI 420) TLS 420 MQ is a highly-refined, Mold Quality stainless steel that is engineered to exhibit excellent polishability, good corrosion resistance, and good wear resistance. TLS 420 MQ is melted using an.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 100 °C |
5.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
Latrobe LSSâ„¢ 420 Supreme Plastic Mold Steel (AISI 420) TLS 420 Supreme is a specially-refined, mold-quality stainless steel that is engineered to provide supreme polishability, good corrosion resistance, and good wear resistance. TLS 420 supreme is manu.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 100 °C |
5.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel TENASTEEL® Cold Work Tool Steel Description: TENASTEEL is a cold work tool steel, combining a high wear resistance together with a very high toughness. Its other advantages are a good machinability in the as-delivery condition and.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 400 °C |
5.67 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec ZN 40 Zirconia, ZrO2-MgO ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 0.000 - 100 °C |
5.67 µin/in-°F @Temperature 32.0 - 212 °F |
|
AK Steel 420 Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 0.000 - 100 °C |
5.67 µin/in-°F @Temperature 32.0 - 212 °F |
|
AK Steel 420 ULTRA HONE® Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 0.000 - 100 °C |
5.67 µin/in-°F @Temperature 32.0 - 212 °F |
|
AK Steel 420HC Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 0.000 - 100 °C |
5.67 µin/in-°F @Temperature 32.0 - 212 °F |
|
AK Steel 420LC Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 100 °C |
5.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum AL 453™ Stainless Steel Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 100 °C |
5.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum AL 468™ Dual Stabilized- Low Titanium Stainless Steel Characteristics:good corrosion resistance in a wide range of environments, can be used in annealed cold formed or as-welded conditions. Applications: used in place of Type 304 in an oxidizing when .. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 100 °C |
5.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 100 °C |
5.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 10% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 100 °C |
5.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 30% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 100 °C |
5.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 70% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 300 °C |
5.67 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG23 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 300 °C |
5.67 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG3 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 10.2 µm/m-°C @Temperature 20.0 - 100 °C |
5.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 50% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |