Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 72.0 µm/m-°C @Temperature 0.000 - 20.0 °C |
40.0 µin/in-°F @Temperature 32.0 - 68.0 °F |
T<Tg; ASTM E831-93 |
Proto3000 Accura® 45HC Plastic Stereolithography (SLA) Prototyping Polymer A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.Benefits:Fast build speed:Provides build speeds that are sign.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature -40.0 - 0.000 °C |
40.0 µin/in-°F @Temperature -40.0 - 32.0 °F |
ASTM E831-00 |
DSM Somos® WaterClear® 10120 Epoxy Resin for Stereolithography
(discontinued **) DescriptionDSM Somos® 10120 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 1.00 - 6.00 mm, Temperature 20.0 °C |
40.0 µin/in-°F @Thickness 0.0394 - 0.236 in, Temperature 68.0 °F |
ASTM D696 |
CPC - Vycom CELTEC® Expanded Rigid foam PVC board Celtec Displayboard is a foamed polyvinyl chloride (PVC) sheet whose combination of features makes it ideal for signage, exhibits, store displays, POP, Kiosks, screen printing and more. The surface.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 50.0 - 200 °C |
40.0 µin/in-°F @Temperature 122 - 392 °F |
DIN 53 752 |
Ensinger TECASINT 4211 SD Polyimide, Black, Carbon Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
Extrusion; ASTM D696 |
Dow STRANDFOAM™ EA 1000 Polypropylene Foam STRANDFOAM™ EA 1000 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibra.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 0.000 - 20.0 °C |
40.0 µin/in-°F @Temperature 32.0 - 68.0 °F |
T<Tg; ASTM E831-93 |
3D Systems Accura® 45HC Plastic for SLA® Systems A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.ApplicationsHigh temperature testing:Automotive "under-the-ho.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 1; Perkin Elmer TMS-2 |
Aptek 6103-A/B Epoxy Encapsulant Optoelectronic grade, reddish black encapsulant for IR LED discreets. Transparent to IR light while blocking out visible light.Part A is deep red. Part B is clear to pale yellow.Information provided.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 1; Perkin Elmer TMS-2 |
Aptek 6108-PMF Epoxy Coating/Encapsulant High temperature, rigid, electrical/electronic coating or encapsulant. Provides excellent environmental protection for continuous exposure to 220°C.Information provided by Aptek Laboratories, Inc. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 1; Perkin Elmer TMS-2 |
Aptek 6108-PMF Epoxy Encapsulant and/or Potting Compound High temperature, rigid, electrical/electronic coating or encapsulant. Provides excellent environmental protection for continuous exposure to 220°C. Also can be used as a high temperature wire varn.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
CTE, linear | 72.0 µm/m-°C @Thickness 0.127 mm |
40.0 µin/in-°F @Thickness 0.00500 in |
second heat; ASTM D 696 |
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |