Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.90 µm/m-°C @Temperature 20.0 - 300 °C |
4.39 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-BAK4 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.90 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.39 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SF5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.90 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.39 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott SF56A Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.90 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.39 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott UG1 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 7.90 µm/m-°C @Temperature 25.0 - 800 °C |
4.39 µin/in-°F @Temperature 77.0 - 1470 °F |
ASTM-C372 |
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
CTE, linear | 7.90 µm/m-°C @Temperature 25.0 - 800 °C |
4.39 µin/in-°F @Temperature 77.0 - 1470 °F |
ASTM-C372 |
CoorsTek ADSR-96R DuraStrate™ 96% Alumina Thick Film Applications: thick films and lasers |
|||
CTE, linear | 7.90 µm/m-°C @Temperature 25.0 - 800 °C |
4.39 µin/in-°F @Temperature 77.0 - 1470 °F |
ASTM-C372 |
CoorsTek Superstrate® 996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
CTE, linear | 7.90 µm/m-°C @Temperature 25.0 - 800 °C |
4.39 µin/in-°F @Temperature 77.0 - 1470 °F |
ASTM-C372 |
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film Applications: thin film substrates |
|||
CTE, linear | 7.90 µm/m-°C @Temperature 30.0 - 800 °C |
4.39 µin/in-°F @Temperature 86.0 - 1470 °F |
|
Ametek Molybdenum-Copper Composite AMC 8020 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |
|||
CTE, linear | 7.90 µm/m-°C @Temperature 20.0 - 600 °C |
4.39 µin/in-°F @Temperature 68.0 - 1110 °F |
|
Advanced Ceramics ACL 1085 (C-795) Alumina Information provided by Advanced Ceramics Limited (ACL) |