Polymer Property : CTE, linear = 36.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 64.8 µm/m-°C

@Temperature 26.0 - 149 °C
36.0 µin/in-°F

@Temperature 78.8 - 300 °F
Diameter
Saint-Gobain Rulon® F Grade Bearing/Seal PTFE
F Grade Bearing/Seal PTFE is used for applications requiring a long wearing material, especially in dry applications and those requiring high abrasion resistance. Standard tape liner material for Ru..