Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 7.07 µm/m-°C

@Temperature 38.0 °C
3.93 µin/in-°F

@Temperature 100 °F
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 538°C
High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer..
CTE, linear 7.07 µm/m-°C

@Temperature 38.0 °C
3.93 µin/in-°F

@Temperature 100 °F
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 593°C
High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer..
CTE, linear 7.07 µm/m-°C

@Temperature 38.0 °C
3.93 µin/in-°F

@Temperature 100 °F
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Annealed Strip/Sheet
High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer..
CTE, linear 7.07 µm/m-°C

@Temperature 38.0 °C
3.93 µin/in-°F

@Temperature 100 °F
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Overaged
High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer..