Polymer Property : CTE, linear = 3.77 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.78 µm/m-°C

@Temperature 30.0 - 150 °C
3.77 µin/in-°F

@Temperature 86.0 - 302 °F
Ametek Tungsten-Copper Composites AWC 8812
Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng..