Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.60 µm/m-°C @Temperature 300 °C |
3.67 µin/in-°F @Temperature 572 °F |
|
MarkeTech Repton EXP 338 Alumina 99.6% EXP 338 features high porosity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cyc.. |
|||
CTE, linear | 6.60 µm/m-°C @Temperature 20.0 - 450 °C |
3.67 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck HPM 1710 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 6.60 µm/m-°C @Temperature 20.0 - 450 °C |
3.67 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck MoCu 80/20 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
CTE, linear | 6.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.67 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott NG1 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG9, NG10, NG11, NG 12 |
|||
CTE, linear | 6.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.67 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott NG5 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG1, NG9, NG10, NG11, NG 12 |
|||
CTE, linear | 6.60 µm/m-°C @Temperature 20.0 - 300 °C |
3.67 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-BK10 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.67 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-KZFS11 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.67 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LAK22 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.60 µm/m-°C @Temperature 20.0 °C |
3.67 µin/in-°F @Temperature 68.0 °F |
Martensitic |
Goodfellow Nickel 55/Titanium 45 Shape Memory Alloy Shape memory alloy is a description applied to that group of metallic materials which show the ability to return to the previously defined shape or size when subjected to the correct thermal procedu.. |
|||
CTE, linear | 6.60 µm/m-°C @Temperature 30.0 °C |
3.67 µin/in-°F @Temperature 86.0 °F |
|
Ceramic Process Systems AlSiC-8, 70 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |
|||
CTE, linear | 6.60 µm/m-°C @Temperature 20.0 - 200 °C |
3.67 µin/in-°F @Temperature 68.0 - 392 °F |
|
CeramTec 848 Zirconia, ZrO2•MgO Tetragonal zirconia exhibits high flexural strength and superior low temperature stability. It features higher impact strength and erosive wear resistance as compared to alumina. 848 TTZP (yellow) i.. |