Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 36.0 µm/m-°C @Temperature 0.000 - 120 °C |
20.0 µin/in-°F @Temperature 32.0 - 248 °F |
100 x 15 x 3 mm sample; AZDEL Test |
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
CTE, linear | 36.0 µm/m-°C @Temperature 0.000 - 120 °C |
20.0 µin/in-°F @Temperature 32.0 - 248 °F |
100 x 15 x 3 mm sample; AZDEL Test |
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |