Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.00 µm/m-°C @Temperature 900 °C |
2.78 µin/in-°F @Temperature 1650 °F |
|
MarkeTech Repton 504 Mullite Brand 504 features: Max spall resistance.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when t.. |
|||
CTE, linear | 5.00 µm/m-°C @Temperature 900 °C |
2.78 µin/in-°F @Temperature 1650 °F |
|
MarkeTech Repton 601 Mullite Brand 601 features: High porosity-low bulk density.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, e.. |
|||
CTE, linear | 5.00 µm/m-°C @Temperature 900 °C |
2.78 µin/in-°F @Temperature 1650 °F |
|
MarkeTech Repton 632 Mullite Brand 632 features: Light Weight Setter.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when th.. |
|||
CTE, linear | 5.00 µm/m-°C @Temperature 900 °C |
2.78 µin/in-°F @Temperature 1650 °F |
|
MarkeTech Repton 663 Mullite Brand 663 features: Zirconia.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycle.. |
|||
CTE, linear | 5.00 µm/m-°C @Temperature 50.0 °C |
2.78 µin/in-°F @Temperature 122 °F |
perpendicular to optical axis |
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam.. |
|||
CTE, linear | 5.00 µm/m-°C @Temperature 20.0 - 450 °C |
2.78 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck HPM 1850W Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.00 µm/m-°C @Temperature 20.0 - 200 °C |
2.78 µin/in-°F @Temperature 68.0 - 392 °F |
|
CeramTec Rubalit® A 1894 Alumina, 94% Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
CTE, linear | 5.00 µm/m-°C @Temperature 0.000 - 100 °C |
2.78 µin/in-°F @Temperature 32.0 - 212 °F |
x direction; IPC TM-650 2.4.24 |
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a.. |