Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.90 µm/m-°C @Temperature 20.0 - 100 °C |
2.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck HPM 1800 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 4.90 µm/m-°C @Temperature 20.0 - 300 °C |
2.72 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck HPM 1850W Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 4.90 µm/m-°C @Temperature 20.0 - 1000 °C |
2.72 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec Rocar® SiF Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
CTE, linear | 4.90 µm/m-°C @Temperature 20.0 - 1000 °C |
2.72 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec Rocar® SiG Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
CTE, linear | 4.90 µm/m-°C @Temperature 30.0 - 400 °C |
2.72 µin/in-°F @Temperature 86.0 - 752 °F |
|
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy) Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif.. |