Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 35.0 µm/m-°C @Temperature <=79.0 °C |
19.4 µin/in-°F @Temperature <=174 °F |
below Tg |
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
CTE, linear | 35.0 µm/m-°C @Temperature -55.0 - 288 °C |
19.4 µin/in-°F @Temperature -67.0 - 550 °F |
Z-Direction; IPC-TM-650 2.4.41 |
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |
|||
CTE, linear | 35.0 µm/m-°C @Temperature -55.0 - 288 °C |
19.4 µin/in-°F @Temperature -67.0 - 550 °F |
Z-Direction; ASTM D3386-94 |
Rogers Corporation RO4535 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a.. |
|||
CTE, linear | 35.0 - 45.0 µm/m-°C @Temperature <=190 °C |
19.4 - 25.0 µin/in-°F @Temperature <=374 °F |
Z-Direction; IPC-TM-650 2.4.24 |
Rogers Corporation Theta® MCL-HE-679G Laminate, GHA-679G Prepreg Halogen-Free, Low Dielectric Constant, High heat Resistant Multi-Layer Circuit Material Theta® circuit materials are halogen free and have good dielectric characteristics suitable for high speed digital applications. Theta materials, in part due to their superior heat resistance, hav.. |
|||
CTE, linear | 35.0 µm/m-°C @Temperature 20.0 °C |
19.4 µin/in-°F @Temperature 68.0 °F |
In machine direction. |
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
CTE, linear | 35.0 µm/m-°C @Temperature 0.000 - 100 °C |
19.4 µin/in-°F @Temperature 32.0 - 212 °F |
FD; ASTM E831 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
CTE, linear | 35.0 µm/m-°C @Temperature <=143 °C |
19.4 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
CTE, linear | 35.0 µm/m-°C @Temperature <=143 °C |
19.4 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica.. |
|||
CTE, linear | 35.0 µm/m-°C @Temperature <=152 °C |
19.4 µin/in-°F @Temperature <=306 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
CTE, linear | 35.0 µm/m-°C @Temperature <=100 °C |
19.4 µin/in-°F @Temperature <=212 °F |
ISO E 830 |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
CTE, linear | 35.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 140 °F |
|
Murtfeldt Murpec® SP Polyetheretherketone Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• .. |