Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 19.5 µm/m-°C @Temperature 1000 °C |
10.8 µin/in-°F @Temperature 1830 °F |
|
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 1000 °C |
10.8 µin/in-°F @Temperature 1830 °F |
|
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
CTE, linear | 19.4 µm/m-°C @Temperature 20.0 - 1000 °C |
10.8 µin/in-°F @Temperature 68.0 - 1830 °F |
|
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
CTE, linear | 19.4 µm/m-°C @Temperature 20.0 - 1000 °C |
10.8 µin/in-°F @Temperature 68.0 - 1830 °F |
|
ATI Allegheny Ludlum 309H Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
CTE, linear | 19.4 µm/m-°C @Temperature 20.0 - 1000 °C |
10.8 µin/in-°F @Temperature 68.0 - 1830 °F |
|
ATI Allegheny Ludlum 309S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
CTE, linear | 19.4 µm/m-°C @Temperature 20.0 - 1000 °C |
10.8 µin/in-°F @Temperature 68.0 - 1830 °F |
|
ATI Allegheny Ludlum 309Si Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 20.0 - 1000 °C |
10.8 µin/in-°F @Temperature 68.0 - 1830 °F |
|
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 25.0 - 1000 °C |
10.8 µin/in-°F @Temperature 77.0 - 1830 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317L (UNS S31703) Allegheny Ludlum's 317L™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless s.. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 25.0 - 1000 °C |
10.8 µin/in-°F @Temperature 77.0 - 1830 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LXN™ (UNS S31726) Allegheny Ludlum's 317LXN™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless.. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 25.0 - 1000 °C |
10.8 µin/in-°F @Temperature 77.0 - 1830 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LX™ (UNS S31725) Allegheny Ludlum's 317LX™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless .. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 20.0 - 700 °C |
10.8 µin/in-°F @Temperature 68.0 - 1290 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 20.0 - 1000 °C |
10.8 µin/in-°F @Temperature 68.0 - 1830 °F |
|
ATI Allegheny Ludlum Type 317 Stainless Steel, UNS S31700 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 20.0 - 700 °C |
10.8 µin/in-°F @Temperature 68.0 - 1290 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 20.0 - 700 °C |
10.8 µin/in-°F @Temperature 68.0 - 1290 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 20.0 - 700 °C |
10.8 µin/in-°F @Temperature 68.0 - 1290 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 20.0 - 700 °C |
10.8 µin/in-°F @Temperature 68.0 - 1290 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 20.0 - 1000 °C |
10.8 µin/in-°F @Temperature 68.0 - 1830 °F |
|
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
CTE, linear | 19.5 µm/m-°C @Temperature 20.0 - 1000 °C |
10.8 µin/in-°F @Temperature 68.0 - 1830 °F |
|
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |