Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 18.2 µm/m-°C @Temperature 500 °C |
10.1 µin/in-°F @Temperature 932 °F |
|
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 500 °C |
10.1 µin/in-°F @Temperature 932 °F |
|
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 1000 °C |
10.1 µin/in-°F @Temperature 1830 °F |
|
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |
|||
CTE, linear | 18.1 µm/m-°C @Temperature 400 °C |
10.1 µin/in-°F @Temperature 752 °F |
|
Outokumpu 4567 Austenitic Stainless Steel Good corrosion resistance with excellent low cold work hardening properties.Applications: Suitable for manufacture of cold headed fasteners.Bar and rod forms. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 500 °C |
10.1 µin/in-°F @Temperature 932 °F |
|
Materion AlBeCastâ„¢ IC910 Aluminum Beryllium Composite Mechanical properties are typical values at RT. AlBeCastâ„¢ IC910 is an aluminum-beryllium alloy that combines the advantages of a net shape casting technology, investment casting, with the stif.. |
|||
CTE, linear | 18.1 µm/m-°C @Temperature 1000 °C |
10.1 µin/in-°F @Temperature 1830 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 20.0 - 1000 °C |
10.1 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 20.0 - 500 °C |
10.1 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 25.0 - 500 °C |
10.1 µin/in-°F @Temperature 77.0 - 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317L (UNS S31703) Allegheny Ludlum's 317L™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless s.. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 25.0 - 500 °C |
10.1 µin/in-°F @Temperature 77.0 - 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LXN™ (UNS S31726) Allegheny Ludlum's 317LXN™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless.. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 25.0 - 500 °C |
10.1 µin/in-°F @Temperature 77.0 - 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LX™ (UNS S31725) Allegheny Ludlum's 317LX™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless .. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 20.0 - 500 °C |
10.1 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 303, Annealed (UNS S30300) Allegheny Ludlum's 303 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 20.0 - 500 °C |
10.1 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum Type 317 Stainless Steel, UNS S31700 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 20.0 - 800 °C |
10.1 µin/in-°F @Temperature 68.0 - 1470 °F |
|
ATI Allegheny Ludlum Stainless Steel AL 904L™ Alloy (UNS N08904) Allegheny Ludlum AL 904 L™ Alloy (UNS N08904) is an austenitic stainless steel alloy designed for a middles to high level of corrosion resistance. The alloy is produced to low carbon levels for us.. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 20.0 - 500 °C |
10.1 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
CTE, linear | 18.2 µm/m-°C @Temperature 20.0 - 500 °C |
10.1 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |