Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 81.0 - 98.0 µm/m-°C @Temperature 90.0 - 150 °C |
45.0 - 54.4 µin/in-°F @Temperature 194 - 302 °F |
T>Tg; ASTM E831-93 |
Proto3000 Accura® Bluestone™ Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features:Exceptional stiffnessHigh temperature resistanceExcellent accuracyHigh humidi.. |
|||
CTE, linear | 81.0 - 98.0 µm/m-°C @Temperature 90.0 - 150 °C |
45.0 - 54.4 µin/in-°F @Temperature 194 - 302 °F |
T>Tg; ASTM E831-93 |
3D Systems Accura® Bluestone™ Plastic for SLA® Systems A high stiffness engineered nanocomposite that opens new applications for stereolithography users. For use with solid-state stereolithography (SLA®) systems.ApplicationsWind-tunnel testing for the .. |