Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 170 - 189 µm/m-°C @Temperature 50.0 - 100 °C |
94.4 - 105 µin/in-°F @Temperature 122 - 212 °F |
ASTM E831-00 |
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look .. |
|||
CTE, linear | 185 - 189 µm/m-°C @Temperature 100 - 150 °C |
103 - 105 µin/in-°F @Temperature 212 - 302 °F |
ASTM E831-00 |
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look .. |
|||
CTE, linear | 170 - 189 µm/m-°C @Temperature 50.0 - 100 °C |
94.4 - 105 µin/in-°F @Temperature 122 - 212 °F |
UV Postcure; ASTM E831-05 |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |
|||
CTE, linear | 185 - 189 µm/m-°C @Temperature 100 - 150 °C |
103 - 105 µin/in-°F @Temperature 212 - 302 °F |
UV Postcure; ASTM E831-05 |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |
|||
CTE, linear | 170 - 189 µm/m-°C @Temperature 50.0 - 100 °C |
94.4 - 105 µin/in-°F @Temperature 122 - 212 °F |
ASTM E831-00 |
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless.. |
|||
CTE, linear | 185 - 189 µm/m-°C @Temperature 100 - 150 °C |
103 - 105 µin/in-°F @Temperature 212 - 302 °F |
ASTM E831-00 |
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless.. |