Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.50 µm/m-°C @Temperature 500 °C |
5.28 µin/in-°F @Temperature 932 °F |
|
Plansee CFY Chromium-Iron-Yttrium The most typical use for CFY is as interconnects in fuel cells.Characteristics: Coefficient of expansion - designed for compatibility with that of the electrolyte in fuel cells Corrosion resistance.. |
|||
CTE, linear | 9.50 - 11.0 µm/m-°C @Temperature 25.0 - 100 °C |
5.28 - 6.11 µin/in-°F @Temperature 77.0 - 212 °F |
|
Materion E20 Beryllium/BeO Composite, 20 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 20.0 - 450 °C |
5.28 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck WCu 70/30 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.28 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott GG475 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG385, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.28 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott WG225 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 20.0 - 300 °C |
5.28 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-BAF51 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.28 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.28 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott RG1000 Long Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 20.0 - 1000 °C |
5.28 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN 51045 |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 20.0 - 300 °C |
5.28 µin/in-°F @Temperature 68.0 - 572 °F |
|
TIMET 75A CP Titanium (ASTM Grade 4) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4901. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specification BS TA. 6.Features.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 20.0 - 300 °C |
5.28 µin/in-°F @Temperature 68.0 - 572 °F |
|
TIMET CP Titanium (ASTM Grade 3) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 538 °C |
5.28 µin/in-°F @Temperature 1000 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 538°C High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 538 °C |
5.28 µin/in-°F @Temperature 1000 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 593°C High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 538 °C |
5.28 µin/in-°F @Temperature 1000 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Annealed Strip/Sheet High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 538 °C |
5.28 µin/in-°F @Temperature 1000 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Overaged High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 20.0 - 300 °C |
5.28 µin/in-°F @Temperature 68.0 - 572 °F |
|
TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1) Commercially Pure Titanium.Industry Specifications: Germany Engineering: 3.7025. Germany Aerospace: 3.7024. France: T-35. UK Aerospace Specification: BS TA. 1.Features: The mechanical properties.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 20.0 - 300 °C |
5.28 µin/in-°F @Temperature 68.0 - 572 °F |
|
TIMET TIMETAL® 50A CP Titanium (ASTM Grade 2) Commercially Pure Titanium.Industry Specifications: USA Aerospace: AMS 4902, 4941. Germany Engineering: 3.7035. Germany Aerospace: 3.7034. France: T-40. UK Aerospace Specifications BS TA. 2, 3,.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 20.0 - 300 °C |
5.28 µin/in-°F @Temperature 68.0 - 572 °F |
|
TIMET TIMETAL® 685 (Ti-6Al-5Zr-0.5Mo-0.25Si) Titanium Alloy High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: Germany Aerospace: 3.7154. France: T-A6ZD. UK Aerospace Specifications BS TA. 43, 44.Features: TIMETAL 685 possesses .. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 21.0 - 300 °C |
5.28 µin/in-°F @Temperature 69.8 - 572 °F |
Mean |
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as an alternative to gray i.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 30.0 °C |
5.28 µin/in-°F @Temperature 86.0 °F |
|
Ceramic Process Systems AlSiC-10, 54 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 25.0 - 200 °C |
5.28 µin/in-°F @Temperature 77.0 - 392 °F |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 843°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 25.0 - 200 °C |
5.28 µin/in-°F @Temperature 77.0 - 392 °F |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 25.0 - 200 °C |
5.28 µin/in-°F @Temperature 77.0 - 392 °F |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 843°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 25.0 - 200 °C |
5.28 µin/in-°F @Temperature 77.0 - 392 °F |
|
Carpenter Hiperco® Alloy 50 Fe-Co-V Soft Magnetic Alloy, Cold Rolled Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 25.0 - 200 °C |
5.28 µin/in-°F @Temperature 77.0 - 392 °F |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |