Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.30 µm/m-°C @Temperature 25.0 - 200 °C |
4.61 µin/in-°F @Temperature 77.0 - 392 °F |
|
Osprey Metals CE7 Al-Si Controlled Expansion Alloy Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 25.0 - 100 °C |
4.61 µin/in-°F @Temperature 77.0 - 212 °F |
|
Osprey Metals CE9 Al-Si Controlled Expansion Alloy Si-40%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 - 100 °C |
4.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck WCu 80/20 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 - 300 °C |
4.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott WG305 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 - 300 °C |
4.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott WG320 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 - 300 °C |
4.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-BK7 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.61 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott SF57 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.61 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott SF57HHT Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.30 - 9.30 µm/m-°C @Temperature 20.0 - 400 °C |
4.61 - 5.17 µin/in-°F @Temperature 68.0 - 752 °F |
|
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The a.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 - 300 °C |
4.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-BAF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 - 1000 °C |
4.61 µin/in-°F @Temperature 68.0 - 1830 °F |
|
CeramTec Rubalit® A 1894 Alumina, 94% Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 25.0 - 1000 °C |
4.61 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM-C372 |
CoorsTek ADS-995 99.5% Alumina Thin Film Applications: thin film substrates |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 25.0 - 1000 °C |
4.61 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM-C372 |
CoorsTek ADS-996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 25.0 - 316 °C |
4.61 µin/in-°F @Temperature 77.0 - 601 °F |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 - 1000 °C |
4.61 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec Rubalit® A 1896 Alumina Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.61 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG20 Band Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BC36 |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 - 1000 °C |
4.61 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec Rubalit® IS 95 Brown Alumina Rubalit® IS 95 brown is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at.. |