Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 7.40 µm/m-°C

@Temperature 20.0 - 50.0 °C
4.11 µin/in-°F

@Temperature 68.0 - 122 °F
PCC-Advanced Forming Technology 68% AlSiC Metal Matrix Composite
AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements ..
CTE, linear 7.40 µm/m-°C

@Temperature 20.0 - 500 °C
4.11 µin/in-°F

@Temperature 68.0 - 932 °F
Misumi Steatite
MgO-SiO2Information provided by MISUMI Corporation.
CTE, linear 7.40 µm/m-°C

@Temperature 20.0 - 300 °C
4.11 µin/in-°F

@Temperature 68.0 - 572 °F
Schott K10 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.40 µm/m-°C

@Temperature 20.0 - 300 °C
4.11 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-BALF4 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.40 µm/m-°C

@Temperature 20.0 - 300 °C
4.11 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-LASF44 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.11 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LASF45 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.11 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LASF9 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.40 µm/m-°C

@Temperature 20.0 - 300 °C
4.11 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-SK4 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.40 µm/m-°C

@Temperature 20.0 - 300 °C
4.11 µin/in-°F

@Temperature 68.0 - 572 °F
Schott P-SF67 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
CTE, linear 7.40 µm/m-°C

@Temperature 20.0 - 300 °C
4.11 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-LAK22 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.11 µin/in-°F

@Temperature -22.0 - 158 °F
Schott BG18 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
CTE, linear 7.40 µm/m-°C

@Temperature 25.0 - 1001 °C
4.11 µin/in-°F

@Temperature 77.0 - 1834 °F
CeramTec 771 94% Alumina (Al2O3)
Te value is 840°C. Hasselman Thermal Shock value is 200 K.Data provided by CeramTec North America.
CTE, linear 7.40 µm/m-°C

@Temperature -200 - 25.0 °C
4.11 µin/in-°F

@Temperature -328 - 77.0 °F
Corning Macor® Machinable Glass Ceramic
The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,..
CTE, linear 7.40 µm/m-°C

@Temperature 30.0 - 800 °C
4.11 µin/in-°F

@Temperature 86.0 - 1470 °F
Ametek Molybdenum-Copper Composite AMC 8515
Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng..
CTE, linear 7.40 µm/m-°C

@Temperature -200 - 25.0 °C
4.11 µin/in-°F

@Temperature -328 - 77.0 °F
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC
Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and ..
CTE, linear 7.40 µm/m-°C

@Temperature 20.0 - 300 °C
4.11 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-KZFS5 Glass
Information Provided by SCHOTT North America, Inc.