Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.07 µm/m-°C @Temperature 38.0 °C |
3.93 µin/in-°F @Temperature 100 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 538°C High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
CTE, linear | 7.07 µm/m-°C @Temperature 38.0 °C |
3.93 µin/in-°F @Temperature 100 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 593°C High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
CTE, linear | 7.07 µm/m-°C @Temperature 38.0 °C |
3.93 µin/in-°F @Temperature 100 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Annealed Strip/Sheet High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
CTE, linear | 7.07 µm/m-°C @Temperature 38.0 °C |
3.93 µin/in-°F @Temperature 100 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Overaged High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |