Polymer Property : CTE, linear = 68.5 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 68.5 µm/m-°C

@Temperature 25.0 - 65.0 °C
38.1 µin/in-°F

@Temperature 77.0 - 149 °F
Alpha 1
Tra-Con Tra-Bond 789-3T3N1 Moisture Resistant Adhesive
TRA-BOND 789-3T3N1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistan..