Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.40 µm/m-°C @Temperature 20.0 - 450 °C |
3.56 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck HPM 1701 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 6.40 µm/m-°C @Temperature 20.0 - 300 °C |
3.56 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck MoCu 80/20 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
CTE, linear | 6.40 µm/m-°C @Temperature 20.0 - 300 °C |
3.56 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 6.40 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.56 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott NG10 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG9, NG1, NG11, NG 12 |
|||
CTE, linear | 6.40 µm/m-°C @Temperature 20.0 - 300 °C |
3.56 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott NG12 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG9, NG10, NG11, NG 1 |
|||
CTE, linear | 6.40 µm/m-°C @Temperature 20.0 - 300 °C |
3.56 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott LAFN7 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.40 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.56 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott NG9 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG1, NG10, NG11, NG 12 |
|||
CTE, linear | 6.40 µm/m-°C @Temperature 20.0 - 300 °C |
3.56 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LAF35 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.40 µm/m-°C @Temperature 25.0 - 200 °C |
3.56 µin/in-°F @Temperature 77.0 - 392 °F |
ASTM-C372 |
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers |
|||
CTE, linear | 6.40 µm/m-°C @Temperature 25.0 - 200 °C |
3.56 µin/in-°F @Temperature 77.0 - 392 °F |
ASTM-C372 |
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
CTE, linear | 6.40 µm/m-°C @Temperature 25.0 - 200 °C |
3.56 µin/in-°F @Temperature 77.0 - 392 °F |
ASTM-C372 |
CoorsTek ADS-995R MidFilm™ 99.5% Alumina Thick Film Applications: thick films and lasers |
|||
CTE, linear | 6.40 µm/m-°C @Temperature 25.0 - 200 °C |
3.56 µin/in-°F @Temperature 77.0 - 392 °F |
ASTM-C372 |
CoorsTek ADSR-96R DuraStrate™ 96% Alumina Thick Film Applications: thick films and lasers |
|||
CTE, linear | 6.40 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.56 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-KZFS5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.40 µm/m-°C @Temperature 20.0 - 200 °C |
3.56 µin/in-°F @Temperature 68.0 - 392 °F |
DIN EN 821-1 |
CeramTec Rubalit® IS 95 Brown Alumina Rubalit® IS 95 brown is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at.. |