Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.40 µm/m-°C @Temperature -30.0 - 70.0 °C |
2.44 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-KZFS2 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 4.40 µm/m-°C @Temperature 20.0 - 600 °C |
2.44 µin/in-°F @Temperature 68.0 - 1110 °F |
DIN EN 821-1 |
CeramTec Rocar® SiG Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
CTE, linear | 4.40 µm/m-°C @Temperature 20.0 - 600 °C |
2.44 µin/in-°F @Temperature 68.0 - 1110 °F |
DIN EN 821-1 |
CeramTec Rocar® ST Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat.. |
|||
CTE, linear | 4.40 µm/m-°C @Temperature 20.0 - 100 °C |
2.44 µin/in-°F @Temperature 68.0 - 212 °F |
ASTM-C372 |
CeramTec Rubalit® 708 Alumina, 96% Based on 96% aluminum oxide, Rubalit® 708 was developed specifically for making heavy-duty resistors and miniature metal layer resistors. Because of its outstanding strength, this same material is .. |
|||
CTE, linear | 4.40 µm/m-°C @Temperature 20.0 - 400 °C |
2.44 µin/in-°F @Temperature 68.0 - 752 °F |
|
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that.. |