Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 30.0 µm/m-°C @Temperature <=143 °C |
16.7 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 50.0 - 200 °C |
16.7 µin/in-°F @Temperature 122 - 392 °F |
DIN 53 752 |
Ensinger TECASINT™ 2031 Polyimide, 40% Graphite Filled (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |