Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Alpase M-5™ Aluminum Mold Plate Excellent weldabilitySurface Condition - Machined top and bottom to reduce costly handling and machining stepsDimensional Stability - High dimensional stability during and after machiningPolishing -.. |