Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 12.7 mm (1/2 in.) thick plate, 1185°C heat treatment, water quenched Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 25.4-50.8 mm forged bar, 1185°C heat treatment, water quenched Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 15% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 30% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 40% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 5% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, GTAW, 3.2 mm sheet Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, investment-cast, as-cast Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, sand cast, 1171°C heat treatment for 2 hours Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 35% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, SMAW, 3.2 mm sheet Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
HP Alloys Alloy 718, 0% Cold Worked, Not Aged 0% Cold Worked, Not Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes .. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
HP Alloys Alloy 718, 15% Cold Worked, Aged 15% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
HP Alloys Alloy 718, 25% Cold Worked, Aged 25% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
HP Alloys Alloy 718, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 12.7-50.8 mm hot-rolled bar, 1185°C heat treatment, water quenched Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 533.4 by 82.55 mm forging, stress relieved at 649°C (1200°F), air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 20% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 23.0 - 700 °C |
9.56 µin/in-°F @Temperature 73.4 - 1290 °F |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 25% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
HP Alloys Alloy 718, 10% Cold Worked, Aged 10% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
HP Alloys Alloy 718, 15% Cold Worked 15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
HP Alloys Alloy 718, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
HP Alloys Alloy 718, 5% Cold Worked 5% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internatio.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
HP Alloys Alloy 718, 5% Cold Worked, Aged 5% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Inte.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
HP Alloys Alloy 718, 20% Cold Worked, Aged 20% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 25.0 - 900 °C |
9.56 µin/in-°F @Temperature 77.0 - 1650 °F |
|
HP Alloys Alloy 718, 25% Cold Worked 25% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |