Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 130 - 140 µm/m-°C @Temperature 25.0 - 300 °C |
72.2 - 77.8 µin/in-°F @Temperature 77.0 - 572 °F |
ASTM D696 |
Polikim EFALON® B-60 PTFE, 60% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
CTE, linear | 130 - 150 µm/m-°C @Temperature 25.0 - 300 °C |
72.2 - 83.3 µin/in-°F @Temperature 77.0 - 572 °F |
ASTM D696 |
Polikim EFALON® K-25 PTFE, 25% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |
|||
CTE, linear | 130 µm/m-°C @Temperature >=150 °C |
72.2 µin/in-°F @Temperature >=302 °F |
ASTM E831 |
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet) KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. .. |
|||
CTE, linear | 130 µm/m-°C @Temperature >=150 °C |
72.2 µin/in-°F @Temperature >=302 °F |
ASTM E831 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |
|||
CTE, linear | 130 µm/m-°C @Temperature >=143 °C |
72.2 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
CTE, linear | 130 µm/m-°C @Temperature >=152 °C |
72.2 µin/in-°F @Temperature >=306 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
CTE, linear | 130 µm/m-°C @Temperature 150 °C |
72.2 µin/in-°F @Temperature 302 °F |
|
Murtfeldt Murpec® Polyetheretherketone In comparison with other thermoplastics, Murpec® has an exceptionally low thermal expansion coefficient. This property provides optimum dimensional stability and means that dimensions do not change.. |
|||
CTE, linear | 130 µm/m-°C @Temperature 100 °C |
72.2 µin/in-°F @Temperature 212 °F |
Estimated by MatWeb from similar grades |
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr.. |