Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.16 µm/m-°C @Temperature 38.0 - 93.0 °C |
7.311 µin/in-°F @Temperature 100 - 199 °F |
|
Latrobe Lescalloy® D6AC VAC-ARC High Strength Alloy Steel LESCALLOY D6AC VAC-ARC steel is a medium carbon, low alloy, ultra high strength steel primarily designed for high strength structural applications requiring strength leaves up to 280,000 psi. This .. |