Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 1200 - 1310 µm/m-°C @Temperature 350 °C |
667 - 728 µin/in-°F @Temperature 662 °F |
|
ChevronTexaco Texatherm® Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging .. |