Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 500 °C |
6.89 µin/in-°F @Temperature 68.0 - 932 °F |
|
International Mold Steel Daido DRM3 Matrix High-Speed Steel This conventional grade MH88 has been improved to DRM3. High hardness and tough DRM3 with excellent hardenability is suitable for high precision cold working tools.Information provided by Internatio.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 200 °C |
6.89 µin/in-°F @Temperature 68.0 - 392 °F |
|
Industeel Superplast® SP300 Prehardened Mold Steel Superplast® 300 (SP300) is a prehardened steel with a BHN 300 (32 HRC) to be used for plastic injection molds, extrusion dies, and compression molds offering improved performance for the mold mak.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 25.0 - 650 °C |
6.89 µin/in-°F @Temperature 77.0 - 1200 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 25.0 - 200 °C |
6.89 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 25.0 - 200 °C |
6.89 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 25.0 - 200 °C |
6.89 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 25.0 - 100 °C |
6.89 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 204 °C |
6.89 µin/in-°F @Temperature 75.2 - 399 °F |
|
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 204 °C |
6.89 µin/in-°F @Temperature 75.2 - 399 °F |
|
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 204 °C |
6.89 µin/in-°F @Temperature 75.2 - 399 °F |
|
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.89 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.89 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 399 °C |
6.90 µin/in-°F @Temperature 68.0 - 750 °F |
|
EDRO #7 Shock Resistant S7 Tool Steel EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 38.0 - 540 °C |
6.89 µin/in-°F @Temperature 100 - 1000 °F |
|
Crucible Compaction Metals CPM® VIM CRU® 20® CPM® VIM CRU® 20® is a vacuum induction melted, cobalt-free super high speed steel manufactured by the Crucible Particle Metallurgy (CPM®) process. VIM CRU processing is designed to meet the cle.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, as welded, notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 204 °C |
6.89 µin/in-°F @Temperature 75.2 - 399 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 204 °C |
6.89 µin/in-°F @Temperature 75.2 - 399 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, SMAW weldment, 19.1 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 25.0 - 100 °C |
6.89 µin/in-°F @Temperature 77.0 - 212 °F |
|
Osprey Metals CE13 Al-Si Controlled Expansion Alloy Al-42%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 204 °C |
6.89 µin/in-°F @Temperature 75.2 - 399 °F |
|
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 204 °C |
6.89 µin/in-°F @Temperature 75.2 - 399 °F |
|
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 204 °C |
6.89 µin/in-°F @Temperature 75.2 - 399 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 24.0 - 93.0 °C |
6.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |