Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.31 µm/m-°C @Temperature 21.0 - 538 °C |
6.839 µin/in-°F @Temperature 69.8 - 1000 °F |
|
Latrobe DuraTechâ„¢ NINE Powder Metal Tool Steel DuraTech NINE is an air-hardening, powder metal tool steel that provides very high wear resistance in combination with high impact toughness. A large volume of hard vanadium carbides provides the hi.. |
|||
CTE, linear | 12.31 µm/m-°C @Temperature 21.0 - 538 °C |
6.839 µin/in-°F @Temperature 69.8 - 1000 °F |
|
Latrobe DuraTech™ A11 Powder Metal Tool Steel (AISI A11) DuraTech A11 powder metal tool steel a versatile air-hardening tool and die steel which provides extremely high wear resistance in combination with relatively high impact toughness. A very large vol.. |