Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 60.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 140 °F |
|
Murtfeldt Murytal® C Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 100 °C |
61.1 µin/in-°F @Temperature 73.4 - 212 °F |
|
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 100 °C |
61.1 µin/in-°F @Temperature 73.4 - 212 °F |
|
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
CTE, linear | 110 - 120 µm/m-°C @Temperature 25.0 - 200 °C |
61.1 - 66.7 µin/in-°F @Temperature 77.0 - 392 °F |
ASTM D696 |
Polikim EFALON® K-25 PTFE, 25% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |
|||
CTE, linear | 110 µm/m-°C @Temperature >=143 °C |
61.1 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
CTE, linear | 110 µm/m-°C @Temperature >=143 °C |
61.1 µin/in-°F @Temperature >=289 °F |
ISO 11359 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
CTE, linear | 110 µm/m-°C @Temperature >=143 °C |
61.1 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
CTE, linear | 110 µm/m-°C @Temperature >=143 °C |
61.1 µin/in-°F @Temperature >=289 °F |
Average above Tg; ASTM D696 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
CTE, linear | 110 µm/m-°C @Temperature >=143 °C |
61.1 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
CTE, linear | 110 µm/m-°C @Temperature >=152 °C |
61.1 µin/in-°F @Temperature >=306 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 200 - 300 °C |
61.1 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ 1750 PTFE Powder
(discontinued **) Type II PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 200 - 300 °C |
61.1 µin/in-°F @Temperature 392 - 572 °F |
ASTM D1530 |
3M Dyneon™ 1620 PTFE Powder
(discontinued **) Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 200 - 300 °C |
61.1 µin/in-°F @Temperature 392 - 572 °F |
ASTM E1530 |
3M Dyneon™ 1641 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 200 - 300 °C |
61.1 µin/in-°F @Temperature 392 - 572 °F |
ASTM E1530 |
3M Dyneon™ 1645 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
CTE, linear | 110 µm/m-°C @Temperature -60.0 - 50.0 °C |
61.1 µin/in-°F @Temperature -76.0 - 122 °F |
DIN 53122 |
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6 Information provided by Arkema Group |
|||
CTE, linear | 110 µm/m-°C @Temperature >=103 °C |
61.1 µin/in-°F @Temperature >=217 °F |
above Tg |
Resinlab® EP1285HD-10 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
CTE, linear | 110 µm/m-°C @Temperature >=34.0 °C |
61.1 µin/in-°F @Temperature >=93.2 °F |
above Tg |
Resinlab® SEC1222 Silver Filled Epoxy Adhesive Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 100 °C |
61.1 µin/in-°F @Temperature 212 °F |
Estimated by MatWeb from similar grades |
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro.. |
|||
CTE, linear | 110 µm/m-°C @Temperature >=143 °C |
61.1 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |
|||
CTE, linear | 110 µm/m-°C @Temperature >=143 °C |
61.1 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |