Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 700 °C |
6.39 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Kennametal Stellite Delcrome® 93 Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 300 °C |
6.39 µin/in-°F @Temperature 68.0 - 572 °F |
|
Kennametal Stellite Stellite® 98M2 cast Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 300 °C |
6.39 µin/in-°F @Temperature 68.0 - 572 °F |
|
Kennametal Stellite Stellite® 98M2 with P/M Processing Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 300 °C |
6.39 µin/in-°F @Temperature 68.0 - 572 °F |
|
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT550 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.0 - 204 °C |
6.39 µin/in-°F @Temperature 69.8 - 399 °F |
|
Latrobe Dynaflex® VAC-ARC High Strength Alloy Steel DYNAFLEX VAC-ARC steel is a medium alloyed, air hardening ultra high strength grade designed for structural applications requiring room temperature tensile strengths of 220,000 to 300,000 psi. Due .. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 427 °C |
6.39 µin/in-°F @Temperature 68.0 - 801 °F |
|
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 427 °C |
6.39 µin/in-°F @Temperature 68.0 - 801 °F |
|
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.1 - 593 °C |
6.40 µin/in-°F @Temperature 70.0 - 1100 °F |
|
Crucible Steel CPM® REX® M35HCHS High Speed Steel, AISI M35 CPM REX M35HCHS is a 5% cobalt modification of M2 high speed steel used almost exclusively for hobs and other gear cutting tools where higher red hardness is required. Made by the Crucible Particle .. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 205 °C |
6.39 µin/in-°F @Temperature 68.0 - 401 °F |
|
Crucible Steel Nu-Die® XL (Premium Quality AISI H13) Tool Steel Nu-Die XL (AISI H13) is a premium version of H13 tool steel manufactured, tested and certified to meet stringent die casting industry specifications issued by NADCA, Chrysler and others. It offers b.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 200 °C |
6.39 µin/in-°F @Temperature 392 °F |
|
Bohler-Uddeholm BÖHLER S400(M7) High Speed Steel Description: High alloyed molybdenum high speed steel with good resistance and high toughness.Applications: Taps, twist drills, reamers, milling tools, broaches tools, cold extrusion dies.Standards:.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 100 °C |
6.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 100 °C |
6.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 200 °C |
6.39 µin/in-°F @Temperature 68.0 - 392 °F |
|
Bohler-Uddeholm BÖHLER W360 ISOBLOC® Hot Work Tool Steel BÖHLER W360 ISOBLOC was developed as a tool steel for dies and punches in warm and hot forging. The steel can be used for a variety of applications where hardness and toughness are required. Prope.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 100 °C |
6.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Ohmaloy® 30 Resistance Alloy Ohmaloy 30 alloy is a moderately magnetic, ductile stainless steel having extremely high electrical resistivity. In addition to imparting high electrical resistivity, the aluminum content in these .. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 427 °C |
6.39 µin/in-°F @Temperature 68.0 - 801 °F |
|
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.1 - 204 °C |
6.40 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.1 - 288 °C |
6.40 µin/in-°F @Temperature 70.0 - 550 °F |
|
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 538 °C |
6.39 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe DuraTech™ 30 Powder Metal High Speed Steel (ASTM M3-2) DuraTech 30 super high speed steel is based upon the chemical composition of ASTM M3-2 high speed steel, but with the addition of over 8% cobalt. DuraTech 30 can be heat treated to 68 HRC. The high .. |