Polymer Property : CTE, linear = 10.72 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 10.72 µm/m-°C

@Temperature 21.0 - 100 °C
5.956 µin/in-°F

@Temperature 69.8 - 212 °F
Carpenter Micro-Melt® 10 Hardened and Tempered Tool Steel (AISI A11)
Micro-Melt® 10 tool steel is a high vanadium tool steel produced using the Carpenter Micro-Melt powder process. This grade possesses wear resistance superior to most other tool steels along with go..
CTE, linear 10.72 µm/m-°C

@Temperature 21.0 - 100 °C
5.956 µin/in-°F

@Temperature 69.8 - 212 °F
Carpenter Micro-Melt® 10 Tough Treated Tool Steel (AISI A11)
Micro-Melt® 10 tool steel is a high vanadium tool steel produced using the Carpenter Micro-Melt powder process. This grade possesses wear resistance superior to most other tool steels along with go..
CTE, linear 10.72 µm/m-°C

@Temperature 21.0 - 100 °C
5.956 µin/in-°F

@Temperature 69.8 - 212 °F
Carpenter Micro-Melt® 10 Wear Treated Tool Steel (AISI A11)
Micro-Melt® 10 tool steel is a high vanadium tool steel produced using the Carpenter Micro-Melt powder process. This grade possesses wear resistance superior to most other tool steels along with go..