Thermal Properties | Metric | English | Comments |
---|---|---|---|
Active Range | 100 - 371 °C | 212 - 700 °F | |
Indium Corp. Indalloy® 84002 Flux #2 Specialty, Acid Based Liquid Flux Indalloy Flux #2 is a specialty acid based liquid flux formulated for the purpose of soldering high chromium containing alloys including stainless steel. Indalloy Flux #2 also has proven to be an e.. |