Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 60.0 - 65.0 µm/m-°C
33.3 - 36.1 µin/in-°F
Average value: 60.8 µm/m-°C Grade Count:6
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
CTE, linear, Transverse to Flow 49.0 - 65.0 µm/m-°C
27.2 - 36.1 µin/in-°F
Average value: 58.0 µm/m-°C Grade Count:4
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
CTE, linear, Transverse to Flow 24.0 - 65.0 µm/m-°C
13.3 - 36.1 µin/in-°F
Average value: 46.1 µm/m-°C Grade Count:8
Overview of materials for Phenolic, Novolac, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values..
CTE, linear, Transverse to Flow 63.0 - 65.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
35.0 - 36.1 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM E 831
SABIC Innovative Plastics LNP Verton RV008ESV PA 66
40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 55.0 - 65.0 µm/m-°C
<br>@Temperature 20.0 °C
30.6 - 36.1 µin/in-°F
<br>@Temperature 68.0 °F
TMA
Vyncolit 4451 XB Novolac Phenolic
Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a..
CTE, linear, Transverse to Flow 65.0 - 65.0 µm/m-°C
<br>@Temperature 160 - 249 °C
36.1 - 36.1 µin/in-°F
<br>@Temperature 320 - 480 °F
Average value: 65.0 µm/m-°C Grade Count:1
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are ..
Copyright © lookpolymers.com All Rights Reserved