Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 70.0 - 130 µm/m-°C | 38.9 - 72.2 µin/in-°F | Average value: 111 µm/m-°C Grade Count:16 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
CTE, linear, Transverse to Flow | 86.4 - 130 µm/m-°C | 48.0 - 72.2 µin/in-°F | Average value: 101 µm/m-°C Grade Count:25 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
CTE, linear, Transverse to Flow | 78.0 - 130 µm/m-°C | 43.3 - 72.2 µin/in-°F | Average value: 103 µm/m-°C Grade Count:3 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
CTE, linear, Transverse to Flow | 68.0 - 130 µm/m-°C | 37.8 - 72.2 µin/in-°F | Average value: 88.6 µm/m-°C Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |