Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 17.0 - 50.0 µm/m-°C | 9.44 - 27.8 µin/in-°F | Average value: 36.3 µm/m-°C Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear, Transverse to Flow | 24.0 - 50.0 µm/m-°C | 13.3 - 27.8 µin/in-°F | Average value: 30.2 µm/m-°C Grade Count:33 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X681 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2920 W Novolac Phenolic Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X682 Novolac Phenolic Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |