Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Temperature 20.0 °C |
7.78 µin/in-°F @Temperature 68.0 °F |
y-axis |
Industrial Laminates/Norplex ES-1 Engraving Stock Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620â€, 0.125â€, and 0.500†|
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Temperature 20.0 °C |
7.78 µin/in-°F @Temperature 68.0 °F |
y-axis |
Industrial Laminates/Norplex ES-2 Engraving Stock Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies. |
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Temperature 20.0 °C |
7.78 µin/in-°F @Temperature 68.0 °F |
y-axis |
Industrial Laminates/Norplex ES-3 Engraving Stock Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin. |
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
7.78 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DEL13PXC PC (Europe-Africa-Middle East) LNP* Stat-kon* DEL13PXC is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Superior Molding. |
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
7.78 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Stat-kon TD000 LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
7.78 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON TD000 PU LNP* STAT-KON* TD000 is an unfilled compound based on Polyurethane resin. Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
7.78 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
7.78 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
7.78 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
7.78 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
7.78 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
7.78 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
CTE, linear, Transverse to Flow | 14.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
7.78 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |